MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crosspolimeri EFRHATAN 72 AM Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Efrhatan: is the trade-mark of our modified polyurethane (PUR).

Efrhatan 72 AM: copolymer TPU(ether base) for MATT technical sheathing extrusion.

Certify: IEC 60332-1

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccISO 1133
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8888ISO 868
Tensile Strength 40.0 MPa5800 psiISO 527
 48.0 MPa
@Temperature 120 °C,
Time 605000 sec
6960 psi
@Temperature 248 °F,
Time 168 hour
Heat Ageing; UL 1581
 48.0 MPa
@Temperature 121 °C,
Time 605000 sec
6960 psi
@Temperature 250 °F,
Time 168 hour
Ageing in oil ASTM II; UL 1581
Elongation at Break 400 %400 %ISO 527
 520 %
@Temperature 120 °C,
Time 605000 sec
520 %
@Temperature 248 °F,
Time 168 hour
Heat Ageing; UL 1581
 520 %
@Temperature 121 °C,
Time 605000 sec
520 %
@Temperature 250 °F,
Time 168 hour
Ageing in oil ASTM II; UL 1581
Tear Strength 90.0 kN/m514 pliambient; DIN 53515
Abrasion 3535[mm³]; DIN 53516
 
Processing PropertiesMetricEnglishComments
Zone 1 155 °C311 °F
Zone 2 165 °C329 °F
Zone 3 175 °C347 °F
Zone 4 180 °C356 °F
Die Temperature 190 °C374 °F
Head Temperature 200 °C392 °F
Dry Time  3.00 hour
@Temperature 90.0 °C
3.00 hour
@Temperature 194 °F
 6.00 hour
@Temperature 90.0 °C
6.00 hour
@Temperature 194 °F
 
Descriptive Properties
Cold Flex-40°CISO 458
Exercise temperature90°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS024 / 294108

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.