Hostacom X M3 T16 G14008 is a 30% talc filled PP copolymer, with medium melt flow rate, high stiffness and medium impact resistance. The product is available in different color matched, pellet form. This grade is delivered in G14008 color version. Applications: Interior TrimsInformation provided by LyondellBasell. |