MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® L 25 G nat 6011 PA12 Film Grade
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Film Grade

Material Notes: Grilamid L 25 G natural 6011 is a high viscosity, lubricated polyamide 12. This product has the following features:
  • Very tasteless
  • High toughness, even at low temperatures
  • Good resistance to weathering
  • Good chemical resistance
  • Mechanical properties only slightly dependent on relative humidity
  • Significantly lower water absorption than polyamide 6
Application examples: Grilamid L 25 G natural 6011 is suitable for the manufacture of blown and cast film being mono or coextruded. Grilamid L 25 G natural 6011 is used for artificial sausage casings for precooked sausages and packaging films for deep-frozen goods.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccDry; ISO 1183
Water Absorption 1.5 %Sim. to ISO 62
Moisture Absorption 0.700 %Sim. to ISO 62
Water Vapor Transmission 8.00 g/m²/day23°C/85% RH; ISO 15106-1/-2
Melt Flow 20 g/10 mincm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 35.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 35.0 MPaISO 527-3
Film Elongation at Break, MD 850 %ISO 527-3
Film Elongation at Break, TD 900 %ISO 527-3
Film Elongation at Yield, MD 6.0 %ISO 527-3
Film Elongation at Yield, TD 6.0 %ISO 527-3
Tensile Modulus 1100 MPaConditioned; ISO 527-1/-2
 1600 MPaDry; ISO 527-1/-2
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
Tear Strength 20.0 kN/mTrouser Tear Resistance, Parallel; ISO 6383-1
 25.0 kN/mTrouser Tear Resistance, Normal; ISO 6383-1
Film Tensile Strength at Break, MD 80.0 MPaISO 527-3
Film Tensile Strength at Break, TD 70.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °CLong Term; ISO 2578
 150 °CShort Term; EMS
 
Optical PropertiesOriginal ValueComments
Gloss 150 %60°; ISO 2813
 
Compliance PropertiesOriginal ValueComments
FDA YesFood contact
 
Descriptive Properties
Carbon Dioxide Transmission Rate, cm³/(m²*d*bar)1500ISO 15105-1/-2; 23°C/0% RH
 1600ISO 15105-1/-2; 23°C/ 85% RH
Elmendorf Tear Resistance, Normal (N)10ISO 6383-2
Elmendorf Tear Resistance, Parallel (N)10ISO 6383-2
EMS Gelboflextest [holes/m²]1300
Food contactEU Requirements
FormGranules
Gelboflextest [holes/m²], EMS1300
Oxygen Transmission Rate, cm³/(m²*d*bar)350ISO 15105-1/-2; 23°C/0% RH
 370ISO 15105-1/-2; 23°C/ 85% RH
PackagingNon oriented film
ProcessingOther Extrusion
Product AttributesHigh viscosity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsan® BESNO MED Nylon 11
EMS-Grivory Grilamid® L 25 nat PA12 Film Grade
EMS-Grivory Grilamid® L 25 nat 6112 PA12
EMS-Grivory Grilamid® L 20 nat PA12
EMS-Grivory Grilamid® L 16 nat PA12

PGRH040 / 156749

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.