MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DSM Biomedical Bionate® 90A Thermoplastic Polycarbonate Polyurethane (PCU)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polyurethane, TP; Polycarbonate-Urethane

Material Notes: A proven family of highly biocompatible medical grade polymers with outstanding physical and mechanical properties Bionate® PCU is a medical grade polymer for use in long-term implants. It has been used in chronically implanted medical devices for nearly two decades. The Bionate® PCU family is one of the most extensively tested families of biomedical polymers and is backed by a comprehensive FDA Master File. Both Bionate® PCU and Bionate® II PCU are tough, biostable and biocompatible polymers with exceptional performance characteristics.

Widely Used The Bionate® PCU family is currently being used in a wide range of applications, including neurostimulation, vascular, artificial heart, cardiac assist and diagnostic devices. Because of its exceptional load-bearing capability and biostability, it is also used extensively in orthopedic applications such as hip and knee joints and spinal motion preservation devices. Due to its biostability, flexibility, electrical properties and tensile strength, the Bionate® PCU family is an excellent candidate for lead insulation.

Tailor Made Bionate® PCU can be modified with SME® technology to incorporate end groups that can enhance device performance. Bionate® II PCU also offers a wide range of potential surface characteristics by using DSM’s patented SAME® technology.

Summary of Product Benefits

  • Biostable and biocompatible
  • Extensively tested
  • Backed by a comprehensive FDA Master File
  • In use for nearly two decades
  • Exceptional abrasion resistance, flexibility and tensile strength
  • Adaptable with SME® and SAME® technology

    Information provided by DSM Biomedical.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 1.20 g/ccASTM D792
    Linear Mold Shrinkage 0.012 in/in4.0 inch Disk; ASTM D955
    Linear Mold Shrinkage, Transverse 0.00 - 0.030 in/inFlame Bar; ASTM D955
    Melt Flow 14 g/10 min
    @Load 1.20 kg,
    Temperature 224 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore A 91ASTM D2240
    Tensile Strength, Ultimate 7993 psiASTM D1708
    Tensile Stress at Strain 1159 psi
    @Strain 50 %
    ASTM D1708
     1604 psi
    @Strain 100 %
    ASTM D1708
     5345 psi
    @Strain 300 %
    ASTM D1708
    Elongation at Break 406 %ASTM D1708
    Flexural Strength 275 psiat 5% deflection; ASTM D790
    Flexural Modulus 6030 psiASTM D790
    Tear Strength 550 pliDie 'C'; ASTM D624
    Taber Abrasion, mg/1000 Cycles 9.1H-18 Wheel; ASTM D1044
     
    Electrical PropertiesOriginal ValueComments
    Dielectric Constant 4.8
    @Frequency 60 Hz
    ASTM D150
    Dielectric Strength 480 V/milASTM D149
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 160.7 µm/m-°C
    @Temperature 20.0 °C
    ASTM E-831
    Vicat Softening Point 88.0 °CASTM D1525
     
    Processing PropertiesOriginal ValueComments
    Processing Temperature 180 - 210 °COptimum Extrusion Conditions
    Rear Barrel Temperature 200 - 215 °C
    Middle Barrel Temperature 193 - 230 °C
    Front Barrel Temperature 193 - 230 °C
    Drying Temperature 82.0 °C
    Dry Time >= 4 hourto moisture < 0.05%
     
    Descriptive Properties
    Acute Systemic ToxicityNo significant systemic toxicity
    Ames MutagenicityNon-mutagenic
    Carcinogenicity: 2 years in ratsNon-carcinogenic
    Chronic Toxicity: USP MuscleMacroscopic reaction not significant
    ColorClear to Amber Pellets
    Complement ActivationLess activation of the complement system
    HemolysisNon-hemolytic
    Humoral Immunological StudyNo humoral (serological) immune
    Intracutaneous ToxicityNo significant irritation or toxicity
    Platelet Deposition (ex vivo shunt)No difference in thrombogenicity
    Sensitization: Magnusson andNo dermal sensitization
    USP Cytotoxicity (MEM Elution)Non-cytotoxic
    USP Implantation Test: 7 daysMacroscopic reaction not significant
    USP PyrogenicityNon-pyrogenic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    DSM Biomedical Bionate® 55D Thermoplastic Polycarbonate Polyurethane (PCU)
    DSM Biomedical Bionate® 80A Thermoplastic Polycarbonate Polyurethane (PCU)
    DSM Biomedical Bionate® II 55D Thermoplastic Polycarbonate Polyurethane (PCU)
    AdvanSource Biomaterials ChronoFlex® AR Biodurable Medical Grade Polyurethane
    AdvanSource Biomaterials ChronoFlex® AL 80A Biodurable Medical Grade Polyurethane

    PBIOS014 / 79728

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.