MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis HB306MO Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: HB306MO is a low melt-flow-rate polypropylene homopolymer intended for compression molding of caps and closures. This grade is designed for the caps and closures market and therefore contains a lubricant for an optimum opening torque of the cap. This grade combines a good balance of stiffness and impact strength with good processability and melt stability. Additives provide anti-static protection. Applications: closures.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ISO 2039-2
Tensile Strength, Yield 39.0 MPaISO 527-2
Elongation at Yield 7.5 %50mm/min; ISO 527-2
Tensile Modulus 1900 MPa1mm/min; ISO 527-2
Charpy Impact, Notched 5.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °CISO 75-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 260 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Copolymer CP0436C30L Calcium Reinforced
Aclo Accutech Polypropylene Homopolymer HP0334C10L Calcium Reinforced
Aclo Accutech Polypropylene CP0437T40V Copolymer Talc Reinforced
Aclo Accutech Polypropylene Copolymer CP0436M30L Mica Reinforced
Aclo Accutech Polypropylene Copolymer CP0436M10L Mica Reinforced

PBOREA465 / 108724

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.