MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® Care ML19 Medical Grade Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Medium viscosity Polyamide 12 for medical application. VESTAMID® Care ML19 is resistant to body fluids and are toxicologically safe.

Features: High bursting strength; Flexible and reliable; High chemical resistance; Low sliding friction; High toughness; Good mechanical properties; Low processing tolerances.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Water Absorption 1.5 %1.5 %Sim. to ISO 62
Moisture Absorption 0.700 %0.700 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inISO 294-4, 2577
Melt Flow 27 g/10 min
@Load 5.00 kg,
Temperature 240 °C
27 g/10 min
@Load 11.0 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.0 MPa6960 psiISO 527
Tensile Strength, Yield 43.0 MPa6240 psiISO 527
Elongation at Break >= 50 %>= 50 %Nominal; ISO 527
 230 %230 %ISO 527
Elongation at Yield 5.0 %5.0 %ISO 527
Tensile Modulus 1.40 GPa203 ksiISO 527
50% Modulus 32.0 MPa
@Strain 50 %
32.0 MPa
@Strain 50 %
ISO 527
Charpy Impact, Notched  0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Complete Break; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 150 µm/m-°C
@Temperature 23.0 - 55.0 °C
83.3 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 178 °C352 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75-1/-2
Vicat Softening Point 140 °C284 °FMethod B: 10 N, 50 K/h; ISO 306
 170 °C338 °FMethod A: 10 N, 50 K/h; ISO 306
Glass Transition Temp, Tg 45.0 °C113 °FISO 11357-1/-2
Flammability Test 1.0
@Thickness 1.60 mm
1.0
@Thickness 0.0630 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK823 / 243032

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.