MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SMAC SMACMOUNT® 2528S Damping Material
Categories: Other Engineering Material

Material Notes: Specifications - Shock & vibration insulation for:
  • Aircraft avionics components & subassemblies
  • Missile electronics
  • Vehicular electronics requiring vibration isolation
Advantages :
  • Bushing style mount
  • Countersunk for lowest installed height
  • Can be pre-loaded to vary natural frequency
  • Axial to radial stiffness ratio of approx. 1:1

Information provided by SMAC MontBlac Groupe Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °CSMACTANE®
 150 °CSMACSIL®
Minimum Service Temperature, Air -55.0 °CSMACSIL®
 5.00 °CSMACTANE®
 
Descriptive Properties
Axial/Radial frequency ratio1/1 approx.
Frequency25-40 Hz
Load0.5 - 3 kgper isolator
MaterialsSMACSIL®
 SMACTANE®
Maximum axial deflection8 mm
Metal partsAluminum and cromated coating
Transmissibility at resonance<2.5SMACTANE®
 <4SMACSIL®
Weight<60 g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SMAC SMACTANE® 60 1114S- N01 Damping Material
SMAC SMACTANE® SP Damping Material
SMAC SMACFOAM® 1250S-02 Damping Material
SMAC SMACFOAM® 1250S-01 Damping Material
SMAC SMACDISK® 1114S Damping Material

PZSMAC030 / 146146

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.