MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Manifattura Cattaneo PEEK Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.

Information provided by Manifattura Cattaneo s.p.a.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 - 1.32 g/ccASTM D792
Moisture Absorption at Equilibrium 0.50 %
@Temperature 23.0 °C
50% RH; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 99ASTM D785
Tensile Strength at Break 94.0 MPaASTM D638
Tensile Strength, Yield 88.0 MPaASTM D638
Elongation at Break 20 - 60 %ASTM D638
Elongation at Yield 5.0 %ASTM D638
Tensile Modulus 3500 MPaASTM D638
Flexural Strength 170 MPaASTM D790
Compressive Strength 122 MPaASTM D695
Poissons Ratio 0.40
Izod Impact, Notched (ISO) 6.10 kJ/m²ASTM D256
Izod Impact, Unnotched (ISO) NBASTM D256
Coefficient of Friction, Dynamic 0.25on polished steel; MPC Test
Coefficient of Friction, Static 0.22on polished steel; MPC Test
K Factor (Wear Factor) 3.9µm/s. PV = 0.1 MPa-m/s; max P = 30 MPa; MPC Test
Limiting Pressure Velocity 1.90 MPa-m/secwithout lubrication; MPC Test
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+13 ohmASTM D257
Dielectric Constant 3.2
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Dielectric Loss Index 0.0030
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 47.0 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.250 W/m-KASTM D177
Maximum Service Temperature, Air 260 °C
Deflection Temperature at 1.8 MPa (264 psi) 160 °CASTM D648-45
Minimum Service Temperature, Air -50.0 °C
Flammability, UL94 V-0
Oxygen Index 24 - 35 %ASTM D2863
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorNatural
UV ResistanceY

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450G™ General Purpose
Solvay APC-2/AS4 PEEK Plus Carbon Fiber Reinforced Unidirectional Tape
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material
Mitsubishi Chemical Advanced Materials Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)
Manifattura Cattaneo PE UMW Polyethylene

PMANIF919 / 156199

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.