MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Anderol ANDEROL® 783-0 Series Synthetic Food Grade Greases, NLGI Grade 0
Categories: Fluid; Lubricant; Aluminum Gellant; Organic Soap Gellant; Polyalphaolefin (PAO)

Material Notes: Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases meet the former H-1 approval requirements of the USDA where incidental food contact can occur. ANDEROL 783 Series Greases are recommended for use with any bearing application, including bottlers, canners, fillers, ways, conveyor systems, centralized lubrication systems and freezers. ANDEROL food grade greases are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. ANDEROL food grade greases are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.” ANDEROL food grade greases also meet the certification requirements recommended by the National Lubricating Grease Institute (NLGI) and the European Lubricating Grease Institute (ELGI).

Information provided by ConocoPhillips.

Anderol® is a registered trademark of The Anderol Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 127Viscosity Index; ASTM D-2270
Saybolt Viscosity at 100°F 200 SUSASTM D-2161
Saybolt Viscosity at 210°F 49 SUSASTM D-2161
Kinematic Viscosity at 40°C (104°F) 39 cStASTM D-445
Kinematic Viscosity at 100°C (212°F) 7.0 cStASTM D-445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.550 mm1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-2266
Penetration P(60), 1/10 mm 355 - 385ASTM D-217
 
Thermal PropertiesOriginal ValueComments
Pour Point -60.0 °FASTM D-97
Flash Point 399 °FASTM D-92
Dropping Point 424 °FASTM D-566
 
Compliance PropertiesOriginal ValueComments
USDA Yes
 
Descriptive Properties
ThickenerAluminum Complex
Water Washout8.1 %ASTM D-1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Anderol ANDEROL® 783-2 Series Synthetic Food Grade Greases, NLGI Grade 2
Anderol ANDEROL® 783-1 Series Synthetic Food Grade Greases, NLGI Grade 1

WCON286 / 75323

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.