MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polikim KESTOIL® Polyamide 6 + Lubricant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Kestoil® is a self-lubricated, strong, wear resistant engineering plastic with a low coefficient of friction. Implicit in its nature, it has many properties that no other material has in combination. It is ideal for bearings without lubrication and for guides. Lubricants and impact and wear resistance increasing additives are added during production to turn Kestamid® into Kestoi®.Integrated into the material, lubricant additives become inseparable and homogenous components. Additives do not leak out even in heaviest operating conditions. Material quality and mechanical machining performance remain unaffected. No oily sensation is felt by touching the surface because additives are spread evenly inside the material.As bearing material, Kestoil® has a wear resistance 5-7 times the standard cast polyamide. This considerable result comes from the fact that the self-lubricating characteristic of the material keeps the coefficient of friction low during operation and thus prevents formation of heat between components that rub against each other. In the absence of self-lubrication, friction is reduced by external lubrication. Yet heat that is formed when lubricant is diminished or totally cleared away shortens material life due to increasing wear.Kestoil® should be preferred in applications where dimensional stability and weatherability of Kestamid® are questionable. As additives fill up pores, humidity and water absorption are reduced; sustaining dimensional stability. As the lubricant additive in Kestoil® is liquid, in high pressure and bearing applications liquid oil may leak out.

Information provided by Polikim Polimer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Water Absorption at Saturation 5.0 %5.0 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383ISO 868
Tensile Strength, Ultimate 73.5 MPa10700 psiISO 527
Elongation at Break >= 30 %>= 30 %ISO 527
Tensile Modulus 4.00 GPa580 ksiISO 527
Compressive Strength 93.2 MPa13500 psiISO 604
Compressive Modulus 2.50 GPa363 ksiISO 604
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²ISO 180
Charpy Impact Unnotched NBNBISO 179
Coefficient of Friction 0.150.15
K Factor (Wear Factor) 0.110.11[mg/km]
K (wear) Factor 120 x 10-8 mm³/N-M59.6 x 10-10 in³-min/ft-lb-hr
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmISO 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmISO 60093
Dielectric Constant 3.73.7ISO 60250
Dielectric Strength 25.0 kV/mm635 kV/inISO 50243
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FISO 11359
Melting Point 220 °C428 °F
Maximum Service Temperature, Air 110 °C230 °Fcontinuous
 170 °C338 °Fshort term

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Tungsten Carbide/Cobalt
Tungsten Carbide, WC
Tungsten Carbide, W2C
Titanium Carbide, TiC
Overview of materials for Acetal Copolymer, Unreinforced

PPOLIK012 / 99822

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.