MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celanex® 2300 GV3/20 PBT, 20% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Chemical abbreviation according to ISO 1043-1: PBT

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %23°C/50%RH; ISO 62
Viscosity Test 82 cm³/g0.82 dl/gISO 307, 1157, 1628
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 250 °C
20 g/10 min
@Load 4.76 lb,
Temperature 482 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psi5mm/min; ISO 527-2/1A
Elongation at Break 4.0 %4.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 3.50 GPa508 ksi50mm/min; ISO 527-2/1A
Flexural Strength 86.0 MPa12500 psiISO 178
Charpy Impact Unnotched 3.40 J/cm²16.2 ft-lb/in²ISO 179/1eU
 3.40 J/cm²
@Temperature -30.0 °C
16.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179/1eA
 0.350 J/cm²
@Temperature -30.0 °C
1.67 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 3500 MPa508000 psiISO 899-1
Tensile Creep Modulus, 1000 hours 2400 MPa348000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
IEC 60250
 4.4
@Frequency 100 Hz
4.4
@Frequency 100 Hz
IEC 60250
Dielectric Strength 26.0 kV/mm660 kV/inIEC 60243-1
Dissipation Factor  0.0085
@Frequency 100 Hz
0.0085
@Frequency 100 Hz
IEC 60250
 0.018
@Frequency 1e+6 Hz
0.018
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 V225 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
Melting Point 225 °C437 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 180 °C356 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FISO 75-1, -2
Vicat Softening Point 190 °C374 °FISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 0.820 mm
HB
@Thickness 0.0323 in
Oxygen Index 21 %21 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Processing Temperature 75.0 - 100 °C167 - 212 °Fcavity
 260 - 270 °C500 - 518 °Fhot runner
Feed Temperature 190 - 200 °C374 - 392 °F
Zone 1 250 - 260 °C482 - 500 °F
Zone 2 250 - 260 °C482 - 500 °F
Zone 3 255 - 265 °C491 - 509 °F
Zone 4 255 - 265 °C491 - 509 °F
Die Temperature 260 - 270 °C500 - 518 °F
Melt Temperature 260 °C500 °FISO 294
 260 - 270 °C500 - 518 °F
Mold Temperature 80.0 °C176 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
Drying Temperature 120 - 140 °C248 - 284 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Hold Pressure 70.0 MPa10200 psiISO 294
Screw Speed  60 rpm
@Diameter 55.0 mm
60 rpm
@Diameter 2.17 in
 75 rpm
@Diameter 40.0 mm
75 rpm
@Diameter 1.57 in
 90 rpm
@Diameter 25.0 mm
90 rpm
@Diameter 0.984 in
 
Descriptive Properties
Injection moldingYes
Injection speedfast
Processing conditions acc. ISO7792

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 3300FC PBT, 30% Glass Reinforced
Celanese Celanex® 2002 PBT, Unfilled
Celanese Celanex® 2001FC PBT, Unfilled
Celanese Celanex® 2001 PBT, Unfilled
Celanese Celanex® 2000-3FC PBT, Unfilled

PHCQ028 / 178483

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.