MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik Sanicro 29 fro OCTG Tube and pipe, seamless
Categories: Metal; Ferrous Metal; Alloy Steel; Austenitic

Material Notes: Sanicro 29 is a high-alloy austenitic stainless steel (CRA) for OCTG down-hole applications in particularly corrosive conditions. The grade is characterized by:
  • Very good resistance to sulphide stress cracking and stress corrosion cracking (SCC) in H2S environments
  • Very high resistance to pitting and crevice corrosion
  • Higher pitting resistance equivalent (PRE) than Sanicro 28 (UNS N08028)
Sanicro 29 is developed specifically for improved localized corrosion resistance where the environment contains high chloride concentrations, CO and H S at high temperatures. Such an environment causes corrosion in lower alloyed materials. Sanicro 29 offers a cost effective solution to such corrosion problems over the more expensive nickel alloys.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C <= 35Sanicro 29-110
 <= 37Sanicro 29-125
Tensile Strength, Ultimate >= 795 MPaSanicro 29-110
 >= 895 MPaSanicro 29-125
Tensile Strength, Yield 760 - 965 MPa
@Strain 0.2 %
Sanicro 29-110
 860 - 1035 MPa
@Strain 0.2 %
Sanicro 29-125
Elongation at Break >= 10 %Sanicro 29-125
 >= 11 %Sanicro 29-110
Modulus of Elasticity 174 GPa
@Temperature 300 °C
 182 GPa
@Temperature 200 °C
 190 GPa
@Temperature 100 °C
 195 GPa
@Temperature 20.0 °C
Poissons Ratio 0.30
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000100 ohm-cm
@Temperature 150 °C
 0.0000100 ohm-cm
@Temperature 200 °C
 0.0000101 ohm-cm
@Temperature 20.0 °C
 0.0000101 ohm-cm
@Temperature 100 °C
 0.0000104 ohm-cm
@Temperature 250 °C
 0.0000111 ohm-cm
@Temperature 300 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µm/m-°C
@Temperature 30.0 - 50.0 °C
 14.5 µm/m-°C
@Temperature 30.0 - 100 °C
 15.0 µm/m-°C
@Temperature 30.0 - 150 °C
 15.0 µm/m-°C
@Temperature 30.0 - 200 °C
 15.0 µm/m-°C
@Temperature 30.0 - 250 °C
 15.0 µm/m-°C
@Temperature 30.0 - 300 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
 0.465 J/g-°C
@Temperature 50.0 °C
 0.480 J/g-°C
@Temperature 100 °C
 0.490 J/g-°C
@Temperature 150 °C
 0.495 J/g-°C
@Temperature 200 °C
 0.505 J/g-°C
@Temperature 250 °C
 0.515 J/g-°C
@Temperature 300 °C
Thermal Conductivity 11.0 W/m-K
@Temperature 20.0 °C
 11.0 W/m-K
@Temperature 50.0 °C
 12.0 W/m-K
@Temperature 100 °C
 13.0 W/m-K
@Temperature 150 °C
 14.0 W/m-K
@Temperature 200 °C
 15.0 W/m-K
@Temperature 250 °C
 16.0 W/m-K
@Temperature 300 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Chromium, Cr 27 %
Copper, Cu 1.0 %
Manganese, Mn <= 2.5 %
Molybdenum, Mo 4.4 %
Nickel, Ni 31.5 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5250 / 199814

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.