MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Formaterm® PS-HI sign/advertising
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Product characteristics:
  • High impact strength and stiffness
  • Very good printable
Product applications:
  • Visual communication
  • Advertising technology

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³DIN EN ISO 1183-1
Water Absorption 0.20 - 0.30 %0.20 - 0.30 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080DIN EN ISO 868
Tensile Strength, Yield 21.0 MPa3050 psiDIN EN ISO 527
Elongation at Break 60 %60 %DIN EN ISO 527
Modulus of Elasticity 1.85 GPa268 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²DIN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmDIN EN 62631-3-1
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmDIN EN 62631-3-2
Dielectric Constant 2.52.5IEC 60250
Dielectric Strength 40.0 kV/mm1020 kV/inIEC 60243
Dissipation Factor 0.00040
@Frequency 1e+6 Hz
0.00040
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C38.9 µin/in-°FDIN 53752
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°FDIN 52612-1
Maximum Service Temperature, Air 80.0 °C176 °Flong term
 90.0 °C194 °Fshort term
Vicat Softening Point 99.0 °C210 °FDIN EN ISO 306, Vicat B
Minimum Service Temperature, Air -10.0 °C14.0 °F
Glass Transition Temp, Tg 95.0 - 100 °C203 - 212 °FISO 11357-3
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 HB
@Thickness 6.00 mm
HB
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis SINKRAL A22V ABS
Versalis EDISTIR N1670 Polystyrene
Versalis EDISTIR N1460 Polystyrene
Stratasys® ABS
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded

PROCH9158 / 232861

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.