MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Radici Radilon® S HSX 100 NT Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: PA6 injection molding grade. Toughened. Natural color. Suitable for parts requiring improved impact resistance.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³DAM; ISO 1183
Water Absorption 9.2 %
@Thickness 2.00 mm,
Time 86400 sec
9.2 %
@Thickness 0.0787 in,
Time 24.0 hour
Immersion @ 23°C; ISO 62
Moisture Absorption 2.70 %
@Thickness 2.00 mm,
Temperature 23.0 °C
2.70 %
@Thickness 0.0787 in,
Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 40.0 MPa5800 psi50mm/min. Conditioned; ISO 527-2/1A
 65.0 MPa9430 psi50mm/min. DAM; ISO 527-2/1A
Elongation at Break 40 %40 %50 mm / min. DAM. Nominal; ISO 527-2/1A
 >= 100 %>= 100 %50 mm / min. Conditioned. Nominal; ISO 527-2/1A
Elongation at Yield 4.1 %4.1 %DAM; ISO 527-2/1A
 20 %20 %Conditioned; ISO 527-2/1A
Tensile Modulus 1.05 GPa152 ksi1mm / min. Conditioned; ISO 527-2/1A
 2.50 GPa363 ksi1mm / min. DAM; ISO 527-2/1A
Flexural Strength 90.0 MPa13100 psi2mm / min. DAM; ISO 178
Flexural Modulus 2.30 GPa334 ksi2mm / min. DAM; ISO 178
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cm1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohm1.00e+12 ohmDAM; 500V.; IEC 60093
Comparative Tracking Index 600 V600 VDAM. Sol.A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FISO 75/2Af
Vicat Softening Point 185 °C
@Load 5.10 kg
365 °F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Flame Spread <= 30.0 mm/min
@Thickness 3.00 mm
<= 1.18 in/min
@Thickness 0.118 in
Automotive Interior; ISO 3795
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 60695-2-1/2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °FInjection Molding
Mold Temperature 70.0 - 80.0 °C158 - 176 °F
 
Descriptive Properties
Injection Molding Injection SpeedMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADI6958 / 293463

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.