Product Description: High heat Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Additive: Flame Retardant Features: Flame Retardant; High Heat Resistance RoSH Compliance: RoSH Compliant Information provided by Chi Mei Corporation |