MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cri-Tech Cri-plastMP F-TPX Fluoro - Thermoplastic Elastomers, After E-beam Crosslinking
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Cri-plast MP F-TPXs are a family of melt processable Fluoro - Thermoplastic Elastomers (F-TPEs) developed to meet a wide range of applications including Automotive, Wire & Cable, & Chemical Industry. Specific grades can be processed by extrusion and injection molding.

Special Features:

  • Thermoplastic processable
  • E-Beam Cross-linkable
  • Excellent flexibility, heat performance & chemical resistance
  • Designed to meet ISO 19642-3 & -5 (600V)
  • Low connector compression set
  • Low permeation
Typical applications:
  • Wire & Cable
  • Fuel and Chemical transfer
  • Tubing/sheet/film

Information provided by Cri-Tech, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 13.8 MPa2000 psi
Elongation at Break 200 %200 %
100% Modulus 10.3 MPa1500 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+8 - 1.00e+9 ohm-cm1.00e+8 - 1.00e+9 ohm-cmWire testing (after water soak); ISO 19642
 1.00e+11 ohm-cm1.00e+11 ohm-cmPlaque testing (dry); ASTM D257

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCRITECH099 / 316308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.