System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Fainplast Compounds Hax™ HF 223F Flame Retardant Polyolefin Cable Compound
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyolefin
;
Polyolefin, Wire/Cable Grade
Material Notes:
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillers
Grade description:
High flexibility, good stress crack resistance
Information provided by Fainplast Compounds
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.45
-
1.49
g/cc
ISO 1183
Melt Flow
3.5
g/10 min
@Load 21.6 kg,
Temperature 150 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Hardness, Shore D
41 - 47
ISO 868
Tensile Strength
11.5
MPa
ISO 527
Elongation at Break
240 %
ISO 527
Electrical Properties
Original Value
Comments
Volume Resistivity
2.00e+15
ohm-cm
ASTM D257
Thermal Properties
Original Value
Comments
Oxygen Index
36 %
ISO 4589
Processing Properties
Original Value
Comments
Processing Temperature
100
-
180
°C
extruder
Shelf Life
3.00
Month
@Temperature 30.0 °C
Moisture absorption after extended storage
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Fainplast Compounds Hax™ HF 224/4 Flame Retardant Polyolefin Cable Compound
Fainplast Compounds Hax™ HFC 0108 Flame Retardant Polyolefin Cable Compound
Fainplast Compounds Hax™ HFX 500S Crosslinkable HFFR Cable Compound
Fainplast Compounds Hax™ HFX 521 Crosslinkable HFFR Cable Compound
Fainplast Compounds Hax™ HFX 505/2 Crosslinkable HFFR Cable Compound
PFAINO908 / 150925
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.