MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
X5CrNiMo18164 Austenitic Stainless Steel for medical instruments
Categories: Metal; Ferrous Metal; Austenitic; Special-Purpose Steel; Stainless Steel

Key Words: medical, surgical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 193 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000740 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.9 µm/m-°C
@Temperature 70.0 - 300 °C
Specific Heat Capacity 0.500 J/g-°C
Thermal Conductivity 16.2 W/m-K
 
Descriptive Properties
Magnetic PropertiesParamagnetic

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
X12CrNi177 Austenitic Stainless Steel for medical instruments
X2CrNiMo17133 Austenitic Stainless Steel for medical instruments
X5CrNi1810 Austenitic Stainless Steel for medical instruments
X5CrNiMo17133 Austenitic Stainless Steel for medical instruments
AISI 316H Stainless Steel, Austenitic

MMEDIC13 / 12389

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.