MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics HVX Silica
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Sintered, fused silica refractory materials with exceptionally low thermal conductivity and thermal expansion. Chemically inert.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 - 2.00 g/cc0.0488 - 0.0723 lb/in³Fired
Porosity 8.0 - 22 %8.0 - 22 %Apparent
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 15.0 - 40.0 MPa
@Temperature 20.0 °C
2180 - 5800 psi
@Temperature 68.0 °F
3-point
Compressive Strength 17.2 MPa2490 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm
@Temperature 20.0 °C
>= 1.00e+14 ohm-cm
@Temperature 68.0 °F
Dielectric Constant 3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.500 µm/m-°C
@Temperature 20.0 °C
0.278 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.900 W/m-K
@Temperature 20.0 °C
6.25 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1000 - 1100 °C1830 - 2010 °Fplus excursions to 1450

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Dioxide, SiO2 (Beta Cristobalite)
Silicon Dioxide, SiO2 (Coesite)
Wacker HDK® H20 Silica
Wacker HDK® N20 Silica
Wacker HDK® T30P Silica

CMORG49 / 90427

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.