MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® B 31 SK 000000 Nylon 6 (PA6), Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: PA 6, non-reinforced, injection molding

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 g/ccISO 60
Density 1.14 g/ccISO 1183
Moisture Absorption at Equilibrium 3.0 %50% RH; ISO 62
Water Absorption at Saturation 10 %ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm150x105x3; 280 °C / MT 80 °C; 400 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cm150x105x3; 280 °C / MT 80 °C; 400 bar; ISO 294-4
Melt Flow 110 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 4647 N
@Temperature 23.0 °C
ISO 6603-2
 6813 N
@Temperature -30.0 °C
ISO 6603-2
Ball Indentation Hardness 150 MPaISO 2093-1
Tensile Strength, Yield 85.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break 10 %50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield 4.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 3500 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 120 MPa2 mm/min; ISO 178-A
Flexural Yield Strength 100 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 3000 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 6.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 115 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
 116 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1eU
 NB
@Temperature -30.0 °C
ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
 <= 10.0 kJ/m²
@Temperature -40.0 °C
ISO 179 1eA
Puncture Energy 46.0 J
@Temperature 23.0 °C
ISO 6603-2
 70.0 J
@Temperature -30.0 °C
ISO 6603-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.0060
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point 222 °C10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 170 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CISO 75-1,-2
Deflection Temperature at 8.0 MPa 50.0 °CISO 75-1,-2
Vicat Softening Point 200 °C
@Load 5.10 kg
120°C/h; ISO 306
 200 °C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-2
@Thickness 3.20 mm
Oxygen Index 25 %Method A; ISO 4589-2
Glow Wire Flammability Index 750 °C
@Thickness 2.00 mm
IEC 60695-2-12
Shrinkage, MD 0.15 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction 150x105x3; ISO 294-4
Shrinkage, TD 0.15 %
@Treatment Temp. 120 °C,
Time 14400 sec
150x105x3; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 °Cinjection molding; ISO 294
 260 - 280 °C
Mold Temperature 80.0 °Cinjection molding; ISO 294
 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 6.00 hour
Moisture Content 0.030 - 0.12 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
JIS SKT4 Low Alloy Tool Steel
JIS SKD11 Tool Steel
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE
AISI 5132H Steel

PLANW9266 / 208067

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.