Sandvik 2RK66 is an austenitic stainless steel alloy suitable for service in medium sour oil and gas environments. It is characterized by: Very good corrosion resistance in Chloride and CO2 containing environments with medium concentrations of H2S at temperatures not exceeding 300oF (150oC) Information provided by Sandvik ASTM 904L; EN 1.4539 |