MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
AIM 47 Fusible Bismuth Alloy
Categories: Metal; Nonferrous Metal; Bismuth Alloy; Solder/Braze Alloy

Material Notes: Uses: low-temperature solder; fixturing delicate parts for machining; lens blocking; proof casting of cavities; dental models; fusible element in safety devices and alarms; radiation blocking for x-rays.

These silvery white alloys expand only ~3.3% of their volume when changing from liquid to solid form, which makes these alloys ideal for many industrial applications. AIM fusible alloys are rarely consumed in an operation and therefore can be remelted and used multiple times. These alloys are normally used in gravity casting but also can be used in other casting methods.

Information provided by AIM Specialty Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 12
Tensile Strength, Ultimate 5400 psi
Elongation at Break 1.5 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000380 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 14.0 J/g
CTE, linear 25.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.0350 BTU/lb-°FLiquid
 0.0350 BTU/lb-°FSolid
Melting Point 47.0 °C
 
Component Elements PropertiesOriginal ValueComments
Bismuth, Bi 44.7 %
Cadmium, Cd 5.3 %
Indium, In 19.1 %
Lead, Pb 22.6 %
Tin, Sn 8.3 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AIM 58 Fusible Alloy
AIM 70 Fusible Alloy
Bi58-Sn42 Bismuth-Tin Eutectic Fusible Alloy
AIM 35.7Sn/35.7Pb/28.6Bi Solder for Photonic Packaging
Bi48-Pb25.63-Sn12.77-Cd9.6 Bismuth-Lead-Tin-Cadmium Fusible Alloy

NAIMSP00 / 14581

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.