MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell CirculenRecover PP300P Grey Polypropylene, Impact Copolymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: CirculenRecover PP300P Grey is a circular polypropylene copolymer supplied in pellet form for injection Molding applications. The grade combines stiffness, impact and flow. The grade is available in grey color sorted from municipal plastic waste.

Sustainability: According with the requirements of Standard ISO 14021:2016, CirculenRecover PP300P Grey contains at least 99 % of recycled material that is fully based on Post-Consumer Waste (PCW) from pre-sorted municipal plastic waste. Filtration level is 150 µm. Volatiles according to ASTM D6980 @ 120 °C are < 0.2%.

This product is not intended for highly regulated applications including food contact, potable water contact, medical and pharmaceutical applications.

Availability: Europe

Application: Containers; Crates; Furniture; Pails

Market: Consumer Products; Rigid Packaging

Processing Method: Injection Molding

Attribute: General Purpose; Good Processability; Impact Copolymer

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.580 g/cc0.0210 lb/in³ISO 60
Density 0.915 g/cc0.0331 lb/in³ISO 1183-1
Melt Flow 16.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
16.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
Ash <= 2.00 %
@Temperature 600 °C
<= 2.00 %
@Temperature 1110 °F
ISO 3451-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 27.0 MPa3920 psiISO 527-1, -2
Elongation at Break 40.0 %40.0 %ISO 527-1, -2
Tensile Modulus 1.30 GPa189 ksiISO 527-1, -2
Charpy Impact, Notched >= 5.00 J/cm²>= 23.8 ft-lb/in²Type 1, Edgewise, Notch A; ISO 179-1/1eA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9055c / 323986

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.