MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Tetrashield™ MP2104 Coating Resin
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Eastman Tetrashield™ protective resin MP2104 for metal packaging enhances the performance of Bisphenol A nonintent (BPA-NI) metal packaging coatings. With high solids, improved retort resistance, and broad chemical resistance, formulations featuring Eastman Tetrashield™ protective resin systems can achieve superior performance results in interior food contact metal packaging applications. Tetrashield MP2104 resin can also be used in ends, caps and closures, and general line applications to improve coating performance in these applications as well as to formulate high solids coating formulations. This resin provides superior functionality for gold phenolic coatings with broad formulation latitude.

Applications

  • Beverage can coatings external
  • Beverage can coatings internal
  • Food can coatings external coatings
  • Food can coatings internal
  • Packaging component - food contact
Key Attributes
  • Chemical resistance
  • Gold phenolic compatibility
  • High solid

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.608 g/cc
Viscosity Test 0.360 dl/g
Molecular Weight 12000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 4.00[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 78.0 °C
 
Descriptive Properties
FormSolid Pellet
Hydroxyl Number15 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4155 / 323778

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.