System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, Carbon Fiber Reinforced
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.
40% Carbon Fiber Reinforced.
The ComAlloy product line has been integrated into the A Schulman product line.
Key Words:
ComAlloy International Company, subsidiary of A. Shulman Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.39
g/cc
Linear Mold Shrinkage
0.0020
cm/cm
ASTM D955
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
120
ASTM D785
Tensile Strength, Ultimate
165
MPa
ASTM D638
Elongation at Break
2.0 %
ASTM D638
Flexural Strength
262
MPa
ASTM D790
Flexural Modulus
14.5
GPa
ASTM D790
Izod Impact, Notched
0.960
J/cm
ASTM D256
Izod Impact, Unnotched
3.74
J/cm
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
149
°C
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
143
°C
ASTM D648
Glass Transition Temp, Tg
145
-
150
°C
Processing Properties
Original Value
Comments
Processing Temperature
310
°C
Approximate middle barrel temperature.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
A. Schulman ComAlloy Hiloy® 515 Polycarbonate, Carbon Fiber Reinforced
A. Schulman ComAlloy Hiloy® 517 Polycarbonate, Carbon Fiber Reinforced
A. Schulman ComAlloy Hiloy® 516 Polycarbonate, Carbon Fiber Reinforced
A. Schulman ComAlloy Hiloy® 716 PPS, Carbon Fiber Reinforced
Akro-Plastic Akrotek® PEEK CF 40 black (5099) PEEK, Conditioned, 30% Carbon Filled
PASH4D / 24920
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.