MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trelleborg B700 Commercial Nitrile Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.

    Properties
  • Good general resistance to oils.
  • Good mechanical properties especially tensile strength, flexing, compression set and impermeability to gases.
  • Moderate aging properties, and good adhesion to metal characteristics.
  • Good adhesion to metal.
  • Moderate resistance to cold.
  • Resistance to Chemicals; good resistance to inorganic chemical products except antioxidant agents and chlorine, and has satisfactory resistance to general hydrocarbons. Being a polar rubber means it is not recommended for use with polar liquids like ketones, ethers and amines. Limited resistance to aromatic hydrocarbons.

All information provided by Trelleborg

Key Words: NBR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.47 g/cc1.47 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070
Tensile Strength, Yield 4.00 MPa580 psi
Elongation at Break 250 %250 %
Tear Strength 15.0 kN/m85.6 pli
Compression Set 45 %
@Temperature 70.0 °C,
Time 79200 sec
45 %
@Temperature 158 °F,
Time 22.0 hour
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 90.0 °C194 °F
Minimum Service Temperature, Air -15.0 °C5.00 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg B800 Commercial Nitrile Rubber
Trelleborg B702 Commercial Nitrile Rubber
Trelleborg B545 High Quality Nitrile Rubber
Trelleborg B500 Commercial Nitrile Rubber
Trelleborg B473 Nitrile Rubber

PTRELL086 / 83844

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.