MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Epoxies, Etc 20-3302NCLV Water Clear Optically Transparent Epoxy Potting Compound & Adhesive
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 20-3302 is a two component, ultra clear epoxy system. It provides excellent optical transmission along with outstanding adhesion and electrical properties. This high purity grade polymer system is formulated with proprietary ultraviolet protectors to minimize yellowing of the cured epoxy. This adhesive\potting compound, when UV aged in a QUV Weatherometer, outperforms other commercially available epoxy systems. 20-3302 is a low viscosity system designed for L.E.D. encapsulating, fiber optics, and any potting or adhesive application requiring optimum clarity. This epoxy system also provides a bubble free and glass smooth finish. 20-3302NCLV is a lower viscosity version of 20-3302. Both resins utilize the same curing agent.

Features:

  • Low viscosity
  • Water clear
  • Outstanding electrical properties
  • Bubble free castings

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccCatalyst
 1.10 g/ccResin
Viscosity 250 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Shear Strength 2250 psiLap
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 3.50e+14 ohm-cm
Dielectric Constant 3.1
Dielectric Strength 500 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 62.0 µm/m-°C
@Temperature 30.0 - 90.0 °C
Maximum Service Temperature, Air 135 °C
Minimum Service Temperature, Air -45.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.564
Transmission, Visible 90 %3000 angstroms
 98 - 99 %3100 angstroms to 2.5 microns
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 hour
@Temperature 125 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 30.0 - 45.0 min
@Load 0.100 kg
 
Descriptive Properties
ColorWater clear
Mix Ratio100:50by weight (Resin:Hardener)
 100:60by volume (Resin:Hardener)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX039 / 316716

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.