Product Description: Film; Characteristics: High clarity, Anti-static, Good resistance chemical Availability: Asia Pacific; Europe; North America Features: Antistatic; Chemical Resistant; High Clarity; Random Copolymer Uses: Film Agency Rating: EC 1907/2006 (REACH); FDA 21 CFR 177.1520© 3.1a RoHS Compliance: RoHS Compliant UL File Number: E162823Information provided by Formosa Chemicals & Fiber Corporation |