MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials Carbo-Rite™ F-1260 Polypropylene, Carbon Black Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with Carbon Black Filler

Material Notes: Product Description: F-1260 is a carbon fiber-reinforced Polyacetal (POM) compound available in pellet form. It solves a wide range of static decay, static shielding and electromagnetic shielding problems. Applications: Machined components; PCB racks
Availability: Asia Pacific, Europe, Latin America, North America
Filler/Reinforcement: Carbon Black
Features: Consistent Performance; Durable; Electromagnetic Shielding (EMI); Rapid Static Decay; Recyclable Material
Uses: Electrical/Electronic Applications; Machine/Mechanical Parts; Racks
Appearance: Black
Forms: Pellets

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ASTM D792
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 58.6 MPa8500 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Tensile Modulus 5.52 GPa800 ksiASTM D638
Flexural Modulus 5.52 GPa800 ksiASTM D790
Izod Impact, Notched 0.481 J/cm
@Thickness 3.17 mm
0.900 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+6 ohm-cm<= 1.00e+6 ohm-cmASTM D257
Surface Resistance <= 1.00e+6 ohm<= 1.00e+6 ohm50% RH; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FUnannealed; ASTM D648
 
Descriptive Properties
Ionic Content11 ng/cm2Anions NO3, Test Method #3010-4
 12 ng/cm2Anions PO4, Test Method #3010-4
 12 ng/cm2Anions Cl, Test Method #3010-4
 14 ng/cm2Anions SO4, Test Method #3010-4
Outgassing<0.03 µg/gMMA, Test Method #3010-3
 0.03 µg/gToluene, Test Method #3010-3
 0.1 µg/gStyrene, Test Method #3010-3
 4 µg/gTotal Organics, Test Method #3010-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR6006 / 268308

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.