MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ascend Performance Materials Vydyne® 67B Nylon 66, Extrusion Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Extruded

Material Notes: Vydyne 67B is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. 67B resin offers high strength, rigidity and toughness over a broad range of demanding applications and good fluid resistance to a wide variety of chemicals, solvents and oils.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DAM; ISO 1183
Water Absorption 8.5 %
@Time 86400 sec
8.5 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 2.5 %2.5 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cm
@Thickness 2.00 mm
0.022 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.021 cm/cm
@Thickness 2.00 mm
0.021 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psiDAM; ISO 527-2
 70.0 MPa10200 psi50% RH; ISO 527-2
Tensile Strength, Yield 55.0 MPa7980 psi50% RH; ISO 527-2
 85.0 MPa12300 psiDAM; ISO 527-2
Elongation at Break 40 %40 %DAM; ISO 527-2
 250 %250 %50% RH; ISO 527-2
Elongation at Yield 5.0 %5.0 %DAM; ISO 527-2
 20 %20 %50% RH; ISO 527-2
Tensile Modulus 1.90 GPa276 ksi50% RH; ISO 527-2
 2.90 GPa421 ksiDAM; ISO 527-2
Flexural Strength 20.0 MPa2900 psi50% RH; ISO 178
 80.0 MPa11600 psiDAM; ISO 178
Flexural Modulus 0.750 GPa109 ksi50% RH; ISO 178
 2.40 GPa348 ksiDAM; ISO 178
Poissons Ratio 0.400.40ISO 527-2
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 30.0 kJ/m²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
55.6 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 260 °C500 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Zone 1 250 - 295 °C482 - 563 °FExtrusion
Zone 2 250 - 295 °C482 - 563 °FExtrusion
Zone 3 250 - 295 °C482 - 563 °FExtrusion
Zone 4 250 - 295 °C482 - 563 °FExtrusion
Zone 5 250 - 295 °C482 - 563 °FExtrusion
Die Temperature 270 - 295 °C518 - 563 °FExtrusion
Melt Temperature 270 - 295 °C518 - 563 °FExtrusion
 
Descriptive Properties
Agency RatingsASTM, D4066 PA0114
 ASTM, D6779 PA0114
 EC, 1935/2004
 EU, 10/2011
 EU, 2023/2006
 FDA, 21 CFR 177.1500
AppearanceNatural Color
FeaturesChemical Resistant
 Gasoline Resistant
 General Purpose
 Good Toughness
 High Melt Stability
 High Rigidity
 High Strength
 High Viscosity
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodOther Extrusion
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SEKISUI SPI ALLEN® 6000 PMMA/ABS
INEOS Styrolution PS 6210/6211 HIPS
INEOS Styrolution PS 5600/5601 HIPS
INEOS Styrolution Lustran® LGM Acrylonitrile Butadiene Styrene (ABS)
INEOS Styrolution Lustran® LGA Acrylonitrile Butadiene Styrene (ABS)

PASCE9764 / 220867

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.