Georgia Gulf 9211 is a food grade vinyl compound designed to maximize clarity. It is suitable for use in a variety of food, cosmetic and personal care products. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |