Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temperatures. Key characteristics: - High stiffness
- High strength
- Good impact strength
- Excellent thermal performance
- Good creep resistance
Information provided by NILIT. |