MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Thermoset™ TC-208 Thermally Conductive Grease
Categories: Fluid; Lubricant

Material Notes: Thermoset TC-208 is a non-reactive, non-silicone, thermally conductive grease with a soft, nonflowable consistency. It is designed for applications where a silicone-free thermal interface material is required and where the device may later need to be easily removed from the heat sink. This formulation is ideally suited for use in thin cross-sectional thicknesses down to < 1 mil. It can be used with a variety of emerging and standard devices in flip chip, PPGA, BGA, and microBGA packages. TC-208 is ideally suited for use on microprocessor, DSP, graphic accelerator and high speed memory devices. Due to its thixotropic nature, TC-208 exhibits low bleed on a wide variety of surfaces and has a successful history of use especially in flip applications.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.46 g/cc
Loss On Ignition <= 0.50 %
@Temperature 150 °C,
Time 86400 sec
 20 %
@Temperature 300 °C,
Time 3600 sec
Viscosity 500000 cP
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.27
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150
 3.31
@Frequency 100000 Hz,
Temperature 25.0 °C
ASTM D150
 3.35
@Frequency 10000 Hz,
Temperature 25.0 °C
ASTM D150
 3.46
@Frequency 1000 Hz,
Temperature 25.0 °C
ASTM D150
Dissipation Factor 0.0101
@Frequency 100000 Hz,
Temperature 25.0 °C
ASTM D150
 0.0128
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150
 0.0201
@Frequency 10000 Hz,
Temperature 25.0 °C
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.20 W/m-KASTM F433
Maximum Service Temperature, Air 85.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 25.0 °C
 
Descriptive Properties
AppearanceWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Syntholube® ISO 32 Compressor Oil
ChevronTexaco TEGRA® ISO 32 Synthetic Compressor Oil
Lord Adhesives Thermoset™ TC-228 Thermally Conductive Grease
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2

PLORD029 / 86037

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.