The flash point is 480°F (249°C). The auto ignition is 662°F (350°C). The ball and ring soft point is 240°F (116°C); ASTM E-28-6-7. The peal strength on canvas is 29 PIW at 72°F (22°C). The bonding range of a 1/8 inch bead on Douglas Fir to Douglas Fir is 40 seconds. The delivery rate is 120 seconds for 1 inch x 3 inch cartridge. Multi-purpose with heat resistance. High performance for many plastics and light gauge metals. Information provided by 3M Adhesives Division. |