MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lion SBR 1686 Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: SBR 1686 is a carbon black master batch (CBMB) based on SBR 1500 latex and N-330 carbon black. It has a low level of oil extension and provides high tensile properties.

Unique Features:

  • Cold polymerized styrene-butadiene elastomer
  • Carbon black master batch
  • Low level extender oil
Applications:
  • Tire treading
  • Conveyor belting and mechanical rubber goods

Information provided by Lion Elastomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D-792
Volatiles <= 0.75 %ZS 1008K
Mooney Viscosity 37 - 57
@Temperature 100 °C
UMS 4+4
Carbon Black Loading 30.6 - 33.6 %
Ash <= 0.50 %
 
Chemical PropertiesOriginal ValueComments
Styrene Content 22.5 - 24.5 %Bound
 
Descriptive Properties
Content<0.5%Soap
 3.1-5.1%Organic acid
 52Carbon black, N-330
Oil10 partsRAE
Polymer100 parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLION039 / 317948

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.