Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Additive: UV Stabilizer Features: Medium Viscosity; UV Resistant Uses: Automotive Applications; Consumer Applications; Electrical/Electronic Applications; Engineering Parts; Hydraulic Applications; Industrial Applications; Pneumatic Applications; Power/Other Tools; Sporting Goods; Tubing; Wire & Cable Applications RoSH Compliance: RoSH Compliant Forms: Granules Processing Method: Extrusion Information provided by EMS-Grivory |