MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
347 Stainless Steel, cold drawn wire, 75% hard, 0.53-3.18 mm diameter
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Niobium plus Tantalum is ten times the minimum carbon content

Key Words: AFNOR Z 6 CNNb 18.10, UNI X 8 CrNiNb 18 11, JIS SUS 347, SS14 2338 (Sweden), UNS S34700, AMS 5512, AMS 5556, AMS 5558, AMS 5571, AMS 5575, AMS 5646, AMS 5654, AMS 5674, AMS 5680, AMS 5681, ASME SA182, ASME SA193, ASME SA194, austenitic, ASME SA213, ASME SA240, ASME SA249, ASME SA312, ASME SA320 (B8C), ASME SA358, ASME SA376, ASME SA403, ASME SA409, ASME SA430, ASME SA473, ASME SA479, ASME SA493, ASME SA511, ASME SA554, ASME SA580, ASME SA633, FED QQ-S-763, FED QQ-S-766, B.S. 347 S 17, B.S. En. 58 F, B.S. En. 58 G, B.S. ANC 3 Grade B, FED QQ-W-423, MIL SPEC MIL-S-862, MIL SPEC MIL-S-23196, SAE J405 (30347), DIN 1.4550, ISO 683/13 16
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1380 - 1585 MPa
Tensile Strength, Yield 1170 - 1380 MPa
@Strain 0.2 %
Elongation at Break 6.0 - 12 %in 50 mm
Modulus of Elasticity 195 GPa
Poissons Ratio 0.27
Fatigue Strength 605 MPa75% hardened specimen
Shear Modulus 77.0 GPa
Izod Impact 120 - 160 J
Charpy Impact 160 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000730 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.3 µm/m-°C
@Temperature 0.000 - 100 °C
 17.8 µm/m-°C
@Temperature 0.000 - 260 °C
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.3 W/m-K
@Temperature 100 °C
 21.5 W/m-K
@Temperature 500 °C
Melting Point 1400 - 1425 °C
Solidus 1400 °C
Liquidus 1425 °C
Maximum Service Temperature, Air 870 °CIntermittent
 925 °CContinuous Service
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 17 %
Iron, Fe 68 %
Manganese, Mn <= 2.0 %
Nb + Ta 0.80 %
Nickel, Ni 11 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
347 Stainless Steel, cold drawn wire, 25% hard, 0.05-0.51 mm diameter
347 Stainless Steel, cold drawn wire, 25% hard, 3.20-9.53 mm diameter
347 Stainless Steel, cold drawn wire, 50% hard, 0.05-0.51 mm diameter
347 Stainless Steel, cold drawn wire, 75% hard, 3.20-9.53 mm diameter
347 Stainless Steel, cold drawn wire, 25% hard, 0.53-3.18 mm diameter

MQ347AH / 12844

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.