MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Viton® A-200 (97.5 phr) Formulation
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Viton was introduced in 1957 as a high-performance aerospace sealing elastomer. It is now also used in other industries including automotive, fluid power, appliance, and chemical industries. It is noted for its outstanding performance in very hot and extremely corrosive environments. Compounds of Viton remain elastic indefinitely at 204°C or when exposed intermittently to 260°C under laboratory conditions. Viton is generally serviceable down to -18 to -23°C, although special formulations permit static use down to -54°C (-65°F). Also, Viton has proven to be satisfactory for static seals under conditions approaching absolute zero. Viton has excellent resistance to oils, fuels, lubricants, and most mineral acids. It has extremely low permeability to a broad range of substances. It is resistant to aliphatic, aromatic hydrocarbons. It is extremely resistant to compression set, even at high temperatures. It has exceptional good resistance to atmospheric oxidation, sun, weather, fungus, and mold. It has good electrical properties in low voltage, low frequency applications and low burning characteristics.

Information provided by manufacturer.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412
Tensile Strength, Ultimate 10.5 MPaCured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412
Elongation at Break 215 %Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412
100% Modulus 0.00520 GPa
@Strain 100 %
Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412
Tear Strength 24.7 kN/mCured 10 min at 177°C and Post Cured 24 hr at 232°C
Compression Set 17 %
@Temperature 200 °C
Method B, O-rings 70 hr; ASTM D1414
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -16.0 °CTemperature Retraction, TR-10; ASTM D1329
Glass Transition Temp, Tg -16.5 °CDSC
 
Descriptive Properties
Formulation as Tested2.5Viton® Curative No. 50
 3High Activity MgO
 30Carbon Black (N-990)
 6Calcium Hydroxide
 97.5Viton® A-200

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Viton® A-200 with Blanc Fixe Fluoroelastomer Compound
Chemours Viton® A-200 with Celite 350 Fluoroelastomer Compound
Chemours Viton® 40 Process Aid
Chemours Viton® 10 Process Aid
Chemours Viton® A-100 with VC50+VC30 Fluoroelastomer Compound

PDVD99 / 33969

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.