MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 4300 G10 50% Glass Filled PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled

Material Notes: Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housings for vehicles, headlamp frames, cams, automotive windscreen wiper arms, PCBs, housings, consoles, contact mounts and covers.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.73 g/cc0.0625 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C; 50% RH
Water Absorption at Saturation 0.40 %0.40 %DIN 53495/1L
Viscosity Measurement  70
@Temperature 290 °C
70
@Temperature 554 °F
20 mins plasticating
 75
@Temperature 280 °C
75
@Temperature 536 °F
30 mins plasticating
 75
@Temperature 300 °C
75
@Temperature 572 °F
10 mins plasticating
 90
@Temperature 270 °C
90
@Temperature 518 °F
30 mins plasticating
 95
@Temperature 290 °C
95
@Temperature 554 °F
10 mins plasticating
 100
@Temperature 260 °C
100
@Temperature 500 °F
30 mins plasticating
 100
@Temperature 300 °C
100
@Temperature 572 °F
5 mins plasticating
 105
@Temperature 280 °C
105
@Temperature 536 °F
10 mins plasticating
 106
@Temperature 250 °C
106
@Temperature 482 °F
30 mins plasticating
 110
@Temperature 270 °C
110
@Temperature 518 °F
10 mins plasticating
 115
@Temperature 260 °C
115
@Temperature 500 °F
10 mins plasticating
 115
@Temperature 240 °C
115
@Temperature 464 °F
30 mins plasticating
 117
@Temperature 250 °C
117
@Temperature 482 °F
10 mins plasticating
 120
@Temperature 240 °C
120
@Temperature 464 °F
10 mins plasticating
Viscosity Test 97 cm³/g0.97 dl/gViscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inSheet
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inSheet
Melt Flow 5.19 g/10 min
@Load 2.16 kg,
Temperature 250 °C
5.19 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 220 MPa
@Load 98.0 kg,
Time 30.0 sec
31900 psi
@Load 216 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength, Yield 140 MPa20300 psi50 mm/min; ISO 527-2
Elongation at Yield 1.5 %1.5 %50 mm/min; ISO 527-2
Modulus of Elasticity 16.0 GPa2320 ksiISO 527-2
Charpy Impact Unnotched  5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 6.90 J/cm²
@Temperature -30.0 °C
32.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Dart Drop, Total Energy 5.00 J3.69 ft-lbW501 housing; ISO 6603-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 93
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 93
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 250
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 250
Dielectric Strength 100 kV/mm2540 kV/inIEC 243/1
Dissipation Factor  0.0012
@Frequency 100 Hz
0.0012
@Frequency 100 Hz
IEC 250
 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 125 V125 VTest solution B; IEC 112
 425 V425 VTest solution A; IEC 112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.40 J/g-°C0.335 BTU/lb-°FIEC 1006
Thermal Conductivity 0.360 W/m-K2.50 BTU-in/hr-ft²-°FDIN 52612
Melting Point 220 - 225 °C428 - 437 °FDSC; ISO 11357-3
Maximum Service Temperature, Air 140 °C284 °Fat 50% loss of tensile strength after 20000h; IEC 216-1
 160 °C320 °Fat 50% loss of tensile strength after 5000h; IEC 216-1
 210 °C410 °F
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FISO 75-2
Decomposition Temperature >= 290 °C>= 554 °F
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Flame Spread <= 100 mm/min<= 3.94 in/minDIN 75200
Glow Wire Test <= 750 °C
@Thickness 3.00 mm
<= 1380 °F
@Thickness 0.118 in
IEC 695
Ignition Temperature 350 °C662 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper Throat
Zone 1 260 °C500 °FFeeding zone
Zone 2 265 °C509 °FCompression
Zone 3 270 °C518 °FMetering-zone
Zone 4 270 °C518 °FNozzle
Melt Temperature 260 °C500 °Ffor shrinkage test
 250 - 275 °C482 - 527 °FInjection-molding
 270 °C518 °FOptimal
Mold Temperature 80.0 °C176 °Ffor shrinkage test, Optimal
 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 - 120 °C176 - 248 °F
Dry Time 4 hour4 hour
 
Descriptive Properties
ColorNatural, Colored, Special Colors and Black
Commercial StatusEurope
Peripheral Screw Speed< 0.25 m/s
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
BASF Ultradur® B 4040 G10 BK5110 50% Glass Filled PBT
Overview of materials for Nylon 6, Extruded
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Direct formed
Overview of materials for Polytetrafluoroethylene (PTFE), Molded

PBASG0093 / 131727

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.