MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Total PPR 7525MZ Polypropylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Clarified random copolymer for injection molding

Clarity - FINA 7525MZ exhibits superior clarity in molded parts.

Impact - FINA 7525MZ produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.

Antistat - FINA 7525MZ contains an antistat to help protect molded parts from dust accumulation.

FDA - FINA 7525MZ complies with all applicable FDA regulations for food contact applications.

Recommended Applications - FINA 7525MZ is recommended for injection molding housewares, cassette cases and other items calling for a combination of good impact, superior clarity and easy mold release.

Processing - FINA 7525MZ resin processes on conventional injection molding equipment with typical melt temperatures of 390-450°F (200-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 10 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90ASTM D288A
Tensile Strength, Ultimate 29.0 MPaASTM D638
Elongation at Break 10 %ASTM D638
Modulus of Elasticity 1.24 GPaASTM D638
Flexural Modulus 1.035 GPaASTM D790
Izod Impact, Notched 0.534 J/cmASTM D256A
Izod Impact, Unnotched NBASTM D256A
Impact Test 15.8 J
@Thickness 3.17 mm
Drop Impact, plaques. Fina API test
 
Thermal PropertiesOriginal ValueComments
Melting Point 149 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 104 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 232 °CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3860X Polypropylene, Extrusion Grade
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene
Formosa Plastics Formolene® 6501A Blow Molding and Injection Molding Polypropylene
Total PPR 8473 Polypropylene, Film Extrusion Grade
Total PPR 7425 Polypropylene, Injection Molding Grade

PFIN96 / 38426

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.