MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Telcar® TL-2417J NAT Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Telcar TL-2417J NAT is a high performance thermoplastic elastomer, available in NAT, designed for a variety of consumer and industrial applications. It is a high density, high hardness, flame retardant grade suitable for extrusion and extrusion coating.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Bondability; Flame Retardant; Good Adhesion; Good Colorability; Good Flow; Good Processability; Good Surface Finish; Good Toughness; High Density; High Hardness; High Specific Gravity

Uses: Consumer Applications; Fabric Coatings; Industrial Applications

RoHS Compliant:RoHS

Form: Pellets

Processing Method: Extrusion; Extrusion Coating

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
15 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  87
@Time 5.00 sec
87
@Time 0.00139 hour
Injection Molded; ASTM D2240
 89
@Time 1.00 sec
89
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 4.32 MPa626 psiAcross Flow, Die C, 20 in/min; ASTM D412
 6.67 MPa968 psiFlow, Die C, 20 in/min; ASTM D412
Tensile Stress at Strain  4.01 MPa
@Strain 300 %
582 psi
@Strain 300 %
Across Flow, Die C, 20 in/min; ASTM D412
 4.04 MPa
@Strain 100 %
586 psi
@Strain 100 %
Across Flow, Die C, 20 in/min; ASTM D412
 5.94 MPa
@Strain 100 %
862 psi
@Strain 100 %
Flow, Die C, 20 in/min; ASTM D412
 6.47 MPa
@Strain 300 %
939 psi
@Strain 300 %
Flow, Die C, 20 in/min; ASTM D412
Elongation at Break 410 %410 %Flow, Die C, 20 in/min; ASTM D412
 800 %800 %Across Flow, Die C, 20 in/min; ASTM D412
Tear Strength 38.7 kN/m221 pliAcross Flow, Die C, 20 in/min; ASTM D624
 51.4 kN/m293 pliFlow, Die C, 20 in/min; ASTM D624
Compression Set  51 %
@Temperature 22.8 °C,
Time 79200 sec
51 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 76 %
@Temperature 70.0 °C,
Time 79200 sec
76 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Zone 1 166 - 188 °C330 - 370 °FExtrusion
Zone 2 171 - 193 °C340 - 380 °FExtrusion
Zone 3 177 - 199 °C350 - 390 °FExtrusion
Zone 4 182 - 204 °C360 - 400 °FExtrusion
Zone 5 182 - 204 °C360 - 400 °FExtrusion
Die Temperature 190 - 210 °C374 - 410 °FExtrusion
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPH 3764 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics and Multifilament Yarns
Top Polymer TPETEX® 7000 TPE
Bamberger Polymers Bapolene® 4042 Polypropylene, Fiber/Filament Grade
3M Nextel™ AF-11 Industrial Woven Fabric 312

PTEKNQ1646 / 238137

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.