Notes: MDF30 is a 30% glass fiber reinforced nylon 6 that offers good mechanical performance coupled with good surface finish. Availability: Europe Fillers/Reinforcement: Glass Fiber, 30% Filler by Weight Features: Good Surface Finish Processing Method: Injection Molding Information provided by Teknor Apex |