MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ChevronTexaco Starplex® Moly NLGI Grade 1
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Texaco Starplex Moly greases deliver value through:
  • Good water resistance — Seals out water, reducing rust and corrosion.
  • Extreme pressure protection.
  • Protection against shock loading — extending vehicle life.
  • Heat resistance with excellent high temperature properties.
  • Good low temperature pumpability — Better low temperature performance means better handling in the container and grease-dispensing equipment.
  • Molybdenum disulfide for additional boundary lubrication protection.

Texaco Starplex Moly greases are multipurpose, water resistant, extreme pressure greases intended primarily for use in construction, mining and agricultural applications.

They are manufactured using selected highly refined high viscosity index base oils, a lithium complex soap, a 1.5% molybdenum disulfide ("moly") antiwear agent, plus oxidation and rust inhibitors. They are dark gray in color and tacky in texture.

Texaco Starplex Moly greases are available in two grades:

  • NLGI 1 for better pumpability at low ambient temperatures
  • NLGI 2 for normal ambient temperatures.

Texaco Starplex Moly greases are designed especially for use in construction, mining and agricultural applications. They can also provide longer mileage life in king pins, spring shackles, and steering system bearings on over-the-road trucks and other offhighway equipment.

Texaco Starplex Moly greases strongly resist being washed out of bearings. They are stable and retain their consistency under adverse service conditions, and protect parts over long service intervals.

Texaco Starplex Moly greases have outstanding film strength and adhesive properties which result in particularly effective protection in shock loadand extreme pressure service. The antiwear properties provided by the lithium complex thickener are enhanced by the molybdenum disulfide. They may also be used in automotive wheel bearing and chassis lubrication.

Texaco Starplex Moly greases are recommended as multipurpose products for the lubrication of both over-the-road and off-highway trucks, tractors, and heavy duty equipment.

They give excellent performance in all automotive equipment in severe service.

They provide top protection to fifth wheels, king pins, wheel bearings, steering system bearings, and all chassis points including ball joints and universal joints.

They also perform well in most heavy-duty industrial applications for general lubrication and for the lubrication of journal bearings, and low and moderate speed antifriction bearings.

They are particularly effective in applications where a high dropping point and high EP are desirable.

They perform well under high temperature, wet, and dusty operating conditions.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 221938; MSDS Number: 8804

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 107107Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 1681 SUS1681 SUSSee Note 3.
Saybolt Viscosity at 210°F 144 SUS144 SUSSee Note 3.
Kinematic Viscosity at 40°C (104°F) 320 cSt320 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 28.5 cSt28.5 cStSee Note 3.
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 315 kg695 lb (mass)
Four Ball Wear 0.500 mm0.0197 inScar Diameter
Penetration P(0), 1/10 mm 301301Unworked, 25°C (77°F)
Penetration P(60), 1/10 mm 315315Unknown Amount of Work, 25°C (77°F)
Timken Test 18100 g40.0 lbOK Load
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °FSee Note 2.
Minimum Service Temperature, Air -34.0 °C-29.2 °FSee Note 1.
Dropping Point 260 °C500 °F
 
Descriptive Properties
ColorDark Gray
Molybdenum Disulfide, wt%1.5
TextureTacky
Thickener, %9Lithium Complex

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WTEXA271 / 77150

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.