MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushion pan/frame to be made of an engineering plastic as opposed to metal. TG7S exhibits improved strength,stiffness and notched impact properties over Ultramid 8333G HI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183
Linear Mold Shrinkage 0.0030 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 170 MPa0.2 in/min; ASTM Test
 77.0 MPa
@Temperature 120 °C
ISO Data
 77.0 MPa
@Temperature 120 °C
ASTM Test
 97.0 MPa
@Temperature 80.0 °C
ASTM Test
 97.0 MPa
@Temperature 80.0 °C
ISO Data
 251 MPa
@Temperature -40.0 °C
ASTM Test
 251 MPa
@Temperature -40.0 °C
ISO Data
Tensile Strength, Ultimate 170 MPa5mm/min; ISO 527
Elongation at Break 3.3 %5mm/min; ISO 527
 3.3 %0.2 in/min; ASTM Test
 3.9 %
@Temperature -40.0 °C
ASTM Test
 3.9 %
@Temperature -40.0 °C
ISO Data
 6.7 %
@Temperature 80.0 °C
ASTM Test
 6.7 %
@Temperature 80.0 °C
ISO Data
 7.0 %
@Temperature 120 °C
ASTM Test
 7.0 %
@Temperature 120 °C
ISO Data
Flexural Strength 260 MPaASTM Test
Flexural Modulus 8400 MPaISO Data
 8970 MPaASTM Test
Izod Impact, Notched 2.25 J/cm
@Thickness 3.17 mm
ASTM Test
Izod Impact, Notched (ISO) 26.0 kJ/m²ISO Test
 18.0 kJ/m²
@Temperature -40.0 °C
ISO Test
Charpy Impact, Notched 2.30 J/cm²ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10 K/min
 220 °CASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 203 °CISO 75
 212 °CASTM Test
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedYes
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® Ultraflow K-FHG8 PA6-GF40, Dry, 40% Glass Filled, Heat Stabilized
Envalior Akulon® K224-G7 PA6-GF35, Dry, 35% Glass Filled
A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6
BASF Ultramid® B3WG7 BK00564 35% Glass Filled PA6 (Dry)
DuPont Mobility and Materials Zytel® 73G40T BK416 PA6-IGF40

PBASF9395 / 85159

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.