MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Idemitsu Kosan XAREC™ SP140 Syndiotactic Polystyrene (SPS), 15% Glass-Filled
Categories: Polymer; Thermoplastic; Polystyrene (PS); Syndiotactic Polystyrene (SPS); Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber

Material Notes: Special grade. PS-ST-GF15.

General Xarec™ Information: XAREC boasts remarkable heat and chemical resistance, as well as superior dimensional stability, making it the preferred SPS in many fields. XAREC is used in the automobile industry for use in critical electrical parts and components. XAREC is often applied to lead-free reflow soldering to comply with current environmental regulations such as RoHS.

Information provided by Idemitsu Losan Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Filler Content 15 %15 %Glass
Moisture Absorption 0.0100 %
@Time 86400 sec
0.0100 %
@Time 24.0 hour
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inIdemitsu Method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inIdemitsu Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.0 MPa10900 psiISO 527
Elongation at Break 2.5 %2.5 %ISO 527
Tensile Modulus 6.50 GPa943 ksiISO 527
Flexural Strength 120 MPa17400 psiISO 178
Flexural Modulus 6.10 GPa885 ksiISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) 29.0 kJ/m²13.8 ft-lb/in²ISO 179
Charpy Impact Unnotched 3.30 J/cm²15.7 ft-lb/in²ISO 179
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 60093
Dielectric Constant 3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 50.0 kV/mm1270 kV/inASTM D149
Dissipation Factor <= 0.0010
@Frequency 1e+6 Hz
<= 0.0010
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index >= 600 V>= 600 VIEC 60112?Solution A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 33.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
18.3 µin/in-°F
@Temperature -22.0 - 86.0 °F
TMA
CTE, linear, Transverse to Flow 71.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
39.4 µin/in-°F
@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °FISO 75B
Deflection Temperature at 1.8 MPa (264 psi) 175 °C347 °FISO 75A
UL RTI, Electrical 50.0 °C122 °FUL746B
UL RTI, Mechanical with Impact 50.0 °C122 °FUL746B
UL RTI, Mechanical without Impact 50.0 °C122 °FUL746B
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 310 °C536 - 590 °F
Mold Temperature 130 - 155 °C266 - 311 °F
Drying Temperature 120 °C
@Time 10800 - 18000 sec
248 °F
@Time 3.00 - 5.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PIDEM153 / 249617

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.