MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sibur ABS 1030 (30,31) Molding Grade ABS Plastic
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: With high fluidity of melting, thermal and light resistance for large parts of devices, parts of refrigerators, and for hearing aids. Mark is allowed for contact with food products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption <= 0.30 %
Melt Index of Compound 20 - 30 g/10 minI Preparation
 <= 30 g/10 minII Preparation
 
Chemical PropertiesOriginal ValueComments
Styrene Content <= 0.050 %
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 17 %II Preparation
 >= 20 %I Preparation
Izod Impact, Notched (ISO) >= 10.0 kJ/m²II Preparation
 >= 12.0 kJ/m²I preparation
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point <= 88.0 °CII Preparation
 <= 90.0 °CI Preparation
 
Optical PropertiesOriginal ValueComments
Gloss 80 %
 
Descriptive Properties
Acrylonitrile Content<.001
Impact Tension Strength>10 MPaPreparation II
 >12 MPaPreparation I

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIB039 / 67602

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.