MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow HDPlas® GNP Plasma Functionalized Graphene Nanoplatelets
Categories: Carbon

Material Notes: Graphene is a carbon based material which is inherently inert and which does not like to mix with, or bond to, other materials. Its excellent properties can only be fully realized when this fundamental hurdle is overcome, and it can be properly dispersed and covalently bonded into matrices such as epoxy resins. HDPlas® GNP have high mechanical strength; high electrical conductivity; high thermal conductivity; and high surface area.

Production process: Source is exfoliated natural graphite; Plasma treatment functionalizes nanomaterial and facilitates dispersion for enhanced application properties.

HDPlas® GNP is also available functionalized with oxygen, nitrogen, ammonia, fluorocarbon, argon, or acid vapor (-COOH).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.215 g/ccEN ISO 60
Particle Size 0.30 - 0.50 µmPlanar Size
Specific Surface Area 20 m²/gBET Analysis
Thickness <= 0.0500 microns
 
Descriptive Properties
Form suppliedDry powder
Graphene Layers10 to 100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Ultra Clean CVD Graphene Film on SiO2/Si Wafers
Goodfellow CVD Graphene Film on Copper Foil
Goodfellow CVD Graphene Film on PET
Goodfellow CVD Graphene Film on Quartz Glass
XG Sciences xGnP® Graphene Nanoplatelets

CGOODF099 / 171685

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.