MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Regalrez™ 1018 Hydrocarbon Resin
Categories: Other Engineering Material

Material Notes: Product Description: Regalrez™ 1018 hydrocarbon resin is produced by polymerization and hydrogenation of pure monomer hydrocarbon feedstocks. Regalrez™ 1018 is a highly stable, light colored, low molecular weight, nonpolar liquid resin suggested for use in plastics modification, adhesives, coatings, sealants, and caulks. Due to its fully hydrogenated cycloaliphatic structure and low softening point Regalrez™ 1018 is useful as a plasticizer in systems where low color and thermal stability are primary concerns and plasticizer migration must be minimized.

Application/Uses:

  • Automotive
  • Building and Construction
  • Caulks and Sealants
  • Hot Melt Adhesives
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Wax Modification
Key Attributes:
  • Excellent thermal and UV stability
  • Fully hydrogenated
  • Highly stable
  • Liquid
  • Water-white color

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1000 cP
@Temperature 60.0 °C
Melt
 10000 cP
@Temperature 40.0 °C
Melt
 100000 cP
@Temperature 30.0 °C
Melt
Molecular Weight 300 g/molMn
 370 g/molMw. Mw/Mn ratio = 1.2
 500 g/molMz
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -23.0 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0ASTM D6166
 
Descriptive Properties
Cloud Point<-40°COMSCP
 20°CDACP
 65°CMMAP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5556 / 222750

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.