MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PoolKemie SILIMOLD AL-25 RTV2 silicon moulding rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Introduction: It is a two component room temperature vulcanizing pour able fluid silicon which cures on the addition of the appropriate CATALYST S o SN, according to the polycondensation process. SILIMOLD AL-25 silicon rubber is characterized by its medium-low hardness and a high tearing resistance. Thanks to these properties, it may also be utilized in the manufacture of moulds with many undercuts.

Application: SILIMOLD AL-25 silicon rubber is ideal in the manufacture of moulds for the production of articles made from synthetic resins (polyester, epoxy polyurethane, etc), plaster, cement, wax etc. It is also suitable for the" wasted wax "process in the artistic casting and founding.

Note 1: Tests have been carried out under these conditions: Temperature: +20°C; After: 24 ore; R.H.: 60%; Catalysis: 100:5

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 - 1.28 g/ccBefore Catalysis
Viscosity 27000 - 33000 cPBefore Catalysis
Linear Mold Shrinkage 0.0050 cm/cmafter 5 days ageing, After Catalysis; ISO 4823
Storage Temperature 5.00 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 22 - 28After Catalysis; DIN 53505
Tensile Strength 5.50 - 6.50 MPaAfter Catalysis; DIN 53504 - S A 3
Elongation at Break 470 - 530 %After Catalysis; DIN 53504 - S A 3
Tear Strength 21.5 - 22.5 kN/mAfter Catalysis; ASTM D 624 S A 3
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourDemoulding time, See note 1, During Catalysis
Pot Life 60.0 - 80.0 minSee note 1, During Catalysis
Shelf Life 12.0 MonthBoth components (A and B) in their original tightly closed containers, in a dry and cool place , away from moisture
 
Descriptive Properties
AppearanceFlexible rubberAfter Catalysis
 Thick LiquidBefore Catalysis
ColorLight greyComponent A, Before Catalysis
 Semi bright whiteAfter Catalysis
 TransparentComponent B, Before Catalysis
Mixing ratio100:5by weight, Before Catalysis
Pouring Time60-80 minSee note 1, During Catalysis

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOOLK002 / 318481

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.