MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

3M Dyneon™ RA 5300 High Performance Rubber Additive
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ Dynamar™ RA 5300 High Performance Rubber Additive is designed for use at low loadings to improve the processing in extrusion and molding operations. It utilizes unique chemistry which makes it particularly effective as a processing aid in fluoroelastomer compounds. Loadings between 0.5 and 1 PHR (parts per hundred rubber) can achieve excellent performance with minimal effect on rheological and physical properties of the overall compound. As a rubber processing additive, Dynamar RA 5300 can help improve the surface finish of FKM extrusions, deliver a higher yield and improve downstream processing. RA 5300 may also aid molding processes with improved flow, release, and tool fouling, especially at higher molding temperatures (approximately 400°F)

    Features and Benefits:
  • High performance rubber additive for fluoroelastomer compounds
  • Provides improved smoothness for FKM extrusions and improved mold release and less mold fouling for molders of FKM compounds compared to typical processing aids
  • Delivers exceptional processing performance with limited property loss
  • Excellent thermal stability
  • Ideal for many FKM tube, profile, and pre-form extrusions, as well as injection and transfer molding processes

Information provided by the Dyneon division of 3M.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity  36.5
@Temperature 121 °C
36.5
@Temperature 250 °F
MS 1+60, Minimum Viscosity
 >= 60
@Temperature 121 °C
>= 60
@Temperature 250 °F
MS 1+60, ts3
 >= 60
@Temperature 121 °C
>= 60
@Temperature 250 °F
MS 1+60, t310
 >= 60
@Temperature 121 °C
>= 60
@Temperature 250 °F
MS 1+60, t318
 77.2
@Temperature 121 °C
77.2
@Temperature 250 °F
MS 1+60, Initial Viscosity
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7171Press Cure 10 Minutes @ 350°C
 7373Heat Age Resistance, 70 Hour @ 270°C
 7474Post Cure 16 Hours @ 232°C
Tensile Strength at Break 9.45 MPa1370 psiPress Cure 10 Minutes @ 350°C
 12.14 MPa1761 psiHeat Age Resistance, 70 Hour @ 270°C
 14.41 MPa2090 psiPost Cure 16 Hours @ 232°C
Elongation at Break 193 %193 %Heat Age Resistance, 70 Hour @ 270°C
 206 %206 %Post Cure 16 Hours @ 232°C
 266 %266 %Press Cure 10 Minutes @ 350°C
100% Modulus  4.39 MPa
@Strain 100 %
637 psi
@Strain 100 %
Press Cure 10 Minutes @ 350°C
 5.43 MPa
@Strain 100 %
788 psi
@Strain 100 %
Heat Age Resistance, 70 Hour @ 270°C
 6.21 MPa
@Strain 100 %
901 psi
@Strain 100 %
Post Cure 16 Hours @ 232°C
Compression Set 13.6 %
@Treatment Temp. 200 °C,
Time 252000 sec
13.6 %
@Treatment Temp. 392 °F,
Time 70.0 hour
-214 O-rings, Aged 70 Hours, 25% Deformation
 
Descriptive Properties
MH, Maximum Toque22.91 inch-lb177°C for 12 Minutes
ML, Minimum Torque1.35 inch-lb177°C for 12 Minutes
t2, Time to 2 Inch-lb Rise from Minimum2.48 Minute177°C for 12 Minutes
t'50, Time to 50% Cure3.04 Minutes177°C for 12 Minutes
t'90, Time to 90% Cure4.24 Minutes177°C for 12 Minutes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDYL9971 / 129989

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.